Forced heat coating system combined with dual separation produces stable pellets, uniform coating, reduced oil absorption and increased resin compatibility. Suitable for Taical resins, recycled pellets and cost-effective applications.
Specifications | Typical value |
---|---|
Production line | Hydraulic crusher – Taiwan technology |
Surface coating technology | Hot stearic acid spray + forced mixing |
Productivity (estimated at THNA) | ~5,000 – 6,000 tons/month |
Average particle size (D50) | 4 – 6 μm |
Maximum particle size (D97) | ≤ 15 μm |
Whiteness (ISO) | ≥ 98% |
Brightness (Hunter L) | ≥ 96% |
CaCO₃ content | ≥ 98.5% |
Stearic acid coverage ratio | 0.8 – 1.2% |
Surface coverage | 97 – 98.5% |
Oil Absorption | 18 – 23 g/100g (reduced compared to uncoated goods) |
Humidity | ≤ 0.20% |
pH | 8.3 – 8.8 |
Dispersion in plastics | Good – suitable for PP, PE, PVC |
Colors | Fine white powder, even color |
Typical applications | Taical plastic, plastic pipes, common plastic granules |
Packaging | PE/PP bag 25kg or Jumbo bag 1,000kg |